Turbolift
- Temperature range of use: –50°C to 140°C
- Available in ordinary lay and Lang‘s lay
- Available in right hand and left hand
- Available in galvanized and ungalvanized
| Diameter Range [mm] | 14 – 56 | 57,15 – 72 |
| RCN | 09 | 11 |
| Number of Outer Strands | 8 | 8 |
| Number of Wires | 311 | 351 |
| Number of Outer Load Bearing Wires | 208 | 248 |
| Average Fill Factor | 0,734 | |
| Average Nominal Metallic Area Factor C | 0,576 | |
| Average Spin Factor | 0,83 | |
Specifications